Download The Development Of An Emat Based In Line Inspection System For The Detection Of Stress Corrosion Cracks In Operating Pipelines PDF/ePub or read online books in Mobi eBooks. Click Download or Read Online button to get The Development Of An Emat Based In Line Inspection System For The Detection Of Stress Corrosion Cracks In Operating Pipelines book now. This website allows unlimited access to, at the time of writing, more than 1.5 million titles, including hundreds of thousands of titles in various foreign languages.
The Development of an EMAT Based In-line Inspection System for the Detection of Stress Corrosion Cracks in Operating Pipelines

This development program was directed to the development of a prototype in-line inspection tool to evaluate the effectiveness of Electromagnetic Acoustic Tranducers (EMATs) for the detection of stress corrosion crack (SCC) development in operating pipelines.
Trends in Oil and Gas Corrosion Research and Technologies

Author: A. M. El-Sherik
language: en
Publisher: Woodhead Publishing
Release Date: 2017-06-09
Trends in Oil and Gas Corrosion Research and Technologies: Production and Transmission delivers the most up-to-date and highly multidisciplinary reference available to identify emerging developments, fundamental mechanisms and the technologies necessary in one unified source. Starting with a brief explanation on corrosion management that also addresses today's most challenging issues for oil and gas production and transmission operations, the book dives into the latest advances in microbiology-influenced corrosion and other corrosion threats, such as stress corrosion cracking and hydrogen damage just to name a few. In addition, it covers testing and monitoring techniques, such as molecular microbiology and online monitoring for surface and subsurface facilities, mitigation tools, including coatings, nano-packaged biocides, modeling and prediction, cathodic protection and new steels and non-metallics. Rounding out with an extensive glossary and list of abbreviations, the book equips upstream and midstream corrosion professionals in the oil and gas industry with the most advanced collection of topics and solutions to responsibly help solve today's oil and gas corrosion challenges. - Covers the latest in corrosion mitigation techniques, such as corrosion inhibitors, biocides, non-metallics, coatings, and modeling and prediction - Solves knowledge gaps with the most current technology and discoveries on specific corrosion mechanisms, highlighting where future research and industry efforts should be concentrated - Achieves practical and balanced understanding with a full spectrum of subjects presented from multiple academic and world-renowned contributors in the industry
AETA 2016: Recent Advances in Electrical Engineering and Related Sciences

These lecture notes present selected topics concerning a wide range of electrical and electronics applications, highlighting innovative approaches and offering state-of-the-art overviews. The book is divided into 14 topical areas, including e.g. telecommunication, power systems, robotics, control systems, renewable energy, mechanical engineering, computer science and more. Readers will find revealing papers on the design and implementation of control algorithms for automobiles and electrohydraulic systems, efficient protocols for vehicular ad hoc networks and motor control, and energy-saving methods that can be applied in various fields of electrical engineering. The book offers a valuable resource for all practitioners who want to apply the topics discussed to solve real-world problems in their challenging applications. Offering insights into common and related subjects in the research fields of modern electrical, electronic and related technologies, it will also benefit all scientists and engineers working in the above-mentioned fields.